Item | Datas |
Color | Color |
Mixture rate | 2:1:0.3 |
Spraying coating | 2-3 layers,40-60um |
Interval of time(20°) | 5-10 minutes |
Drying time | Surface dry 45 minutes, polished 15 hours. |
Available time (20°) | 2-4 hours |
Spraying and applying tool | Geocentric spray gun(upper bottle) 1.2-1.5mm;3-5kg/cm² |
Suction spray gun(lower bottle) 1.4-1.7mm; 3-5kg/cm² | |
Theory quantity of paint | 2-3 layers about 3-5㎡/L |
Film Thickness | 30~40 micrometer |
1. Low VOC content with low viscosity. Cures quickly and low reduction on curing.
2. Allow smooth flow out after with rheological properties. The ability to be polished and sanded in refinish applications.
3. Time reduction in clearing coat application with the help of film formation.
Automotive refinish coatings enhances the appearance of vehicles and also improves their durability, along with growing demand for recreational vehicles and increase in the number of vehicle collisions on a large scale
There are a number of reasons why a car’s paint job might need refinishing. The paint can be peeling, or the car could be rusted or have some other type of body damage. If you want to refinish the paint so it looks like new, you can’t just apply a new coat over the old one. This is a complex process involving sanding over the surface and making sure it is completely smooth, and shouldn’t be taken on by someone inexperienced in car painting.
Step 1
Clean the entire surface with water, then use a wax/grease remover. Make sure you remove all wax, grease and other forms of contamination from the old finish.
Step 2
Cover all surfaces and panels of the car that are not being refinished, using tarp, masking tape or other materials that will completely mask those areas.
Step 3
Remove all rust from the surface. You might be able to remove small traces of rust . If there is larger, more significant rust, you may need to cut that metal away and then weld patches of 22- to 18-gauge metal using a wire-feed welding torch.
Step 4
Repair any dents in the panel. “Pull” or pound the dent back out using either a hammer from the inside or a suction cup with a handle on the outside. If there are large dents and you want a perfect surface, you’re better off having the whole panel replaced.
Step 5
Sand down all the paint that remains on that panel. Rub the surface with 320-grit sandpaper until the old paint is smooth with no rough areas. If the paint’s top coat is peeling, remove all the paint from the panel; a power sander might be needed for this.
Step 6
Primer the surface, whether it is bare metal or still has layers. Apply polyurethane primer to the entire surface, then block the primer by wrapping 400-grit sandpaper around a ridged block and running it against the surface to smooth out the primer and remove any gloss.
Step 7
Double-check to make sure the surface is completely clean and dry, that all surfaces not being refinished are masked and covered, then apply the top coat of paint, preferably with a good paint gun, using even strokes. If you are painting bare metal, apply two coats 15 minutes apart.
Apply three clear coats after the new top coat is dry, waiting 15 minutes between coats for the previous coat to dry.
Automotive refinish coatings has 1L,2L,3L,4L,5L package, if you want to use others size, you contact us, we would like to supply customized service.
Transport and storage
1. The product should be stored in a cool and ventilated place to prevent direct sunlight, and keep it away from fire sources.
2. When the product is being transported, it should be protected from rain and sunlight, avoid collisions, and comply with the relevant regulations of the transportation department.
International express
For sample order, we’ll suggest you shipping by DHL, TNT or air shipping. They are the most fast and convenient shipping ways. To keep the goods in good condition, there will be wood frame outside the carton box.
Sea shipping
1, For LCL shipment volume over 1.5CBM or full container, we’ll suggest you shipping by sea. It is the most economical mode of transport.
2, For LCL shipment, normally we will put all the goods standing on the pallet, besides, there will be plastic film wrapped outside the goods.